Patti
The polish is made to do the work, really don't need to apply a whole lot
of pressure. Remember the various tests when it comes to polishing - the
1, 5, and 10 foot tests. For it to look good at ten feet away takes a
certain amount of work, the 5 foot test probably takes about 2x as much
work. The 1 foot test takes about 10x the amount of work. Those pock
marks may take forever to polish out. That pitting is common in the old
trailers and is very hard to get out, if at all, completetly.
Also, be careful about using too much polish - don't know if you remember
Herbs demonstration at the VAC rally, just need to put little dots - too
much polish starts working against you.